Film blowing of silane-modified polyethylene
2009
The grafting of vinyltriethoxysilane (VTES) onto polyethylene (PE) with the help of small amounts of peroxides was investigated to film-blow these modified materials. The degree of crosslinking was kept very low to achieve good melt processability and improved mechanical properties. The possibility of obtaining modified PE films with improved properties and regularly distributed crosslinking with a single processing step demonstrates the uniqueness of this study. The additive concentration was established through preliminary studies; with a batch mixer, it was possible to process the modified PE in the film-blowing operation. Water treatment of the modified films after film blowing allowed …
Structure-property relationships of polycarbonate diol-based polyurethanes as a function of soft segment content and molar mass
2014
Segmented thermoplastic polyurethanes (PUs) have been synthesized with polycarbonate diol as soft segment and 4,4′-diphenylmethane diisocyanate and butanediol as hard segment. Two different series employing two different soft-segment molar mass, 1000 and 2000 g/mol, and by changing the hard-segment content from 32 to 67% have been investigated with the aim to elucidate the effect of the different content variations on the properties. Morphological, thermal, and mechanical properties have been studied by Fourier transform infrared spectroscopy (FTIR), differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), wide angle X-ray diffraction, atomic force microscopy, tensile and…